Specs Magnets Earth Rare

Samarium KobaltMagnetNîşan û Taybetmendî:

Magneta Samarium Kobalt (SmCo) jî wekî magneta Kobaltê ya erdê hindik tê gotin. Berxwedana wê ya bilind a li hember demagnetîzasyonê û aramiya germahiya hêja dihêle ku magneta germahiya bilind SmCo an magneta Sm2Co17 di bin germahiya bilind a 350 °C de aram bixebite. Bi gelemperî cilê ne hewce ye. Ji ber vê yekê magneta SmCo ji bo gelek serîlêdanên performansa bilind ên wekî pîşesaziyên hewayê, motorspor û otomotîvê vebijarkek premium a materyalê magnet e.

Sinif Induction Bermayî
Br
Coercivity
Hcb
Zordariya Navxweyî
Hcj
Hilbera Enerjiya herî zêde
(BH) max
Rev. Temp. Coef.
α(Br)
Rev. Temp. Coef.
β(Hcj)
Max Working Temp.
T kG kA/m kOe kA/m kOe kJ/m3 MGOe %/°C %/°C °C
magnets SmCo5, (SmPr)Co5, SmCo 1:5
YX14 0,74-0,80 7.4-8.0 573-629 7.2-7.9 >1194 >15 96-119 12-15 -0.04 -0.30 250
YX14H 0,74-0,80 7.4-8.0 573-629 7.2-7.9 >1592 >20 96-119 12-15 -0.04 -0.30 250
YX16 0,79-0,85 7,9-8,5 612-660 7.7-8.3 >1194 >15 110-135 14-17 -0.04 -0.30 250
YX16H 0,79-0,85 7,9-8,5 612-660 7.7-8.3 >1592 >20 110-135 14-17 -0.04 -0.30 250
YX18 0,84-0,90 8.4-9.0 644-700 8.1-8.8 >1194 >15 127-151 16-19 -0.04 -0.30 250
YX18H 0,84-0,90 8.4-9.0 644-700 8.1-8.8 >1592 >20 127-151 16-19 -0.04 -0.30 250
YX20 0,89-0,94 8.9-9.4 676-725 8.5-9.1 >1194 >15 143-167 18-21 -0.04 -0.30 250
YX20H 0,89-0,94 8.9-9.4 676-725 8.5-9.1 >1592 >20 143-167 18-21 -0.04 -0.30 250
YX22 0,92-0,96 9.2-9.6 710-748 8.9-9.4 >1194 >15 160-183 20-23 -0.04 -0.30 250
YX22H 0,92-0,96 9.2-9.6 710-748 8.9-9.4 >1592 >20 160-183 20-23 -0.04 -0.30 250
YX24 0,95-1,00 9,5-10,0 730-780 9.2-9.8 >1194 >15 175-199 22-25 -0.04 -0.30 250
YX24H 0,95-1,00 9,5-10,0 730-780 9.2-9.8 >1592 >20 175-199 22-25 -0.04 -0.30 250
magnets Sm2Co17, Sm2(CoFeCuZr)17, SmCo 2:17
YXG22 0,93-0,97 9.3-9.7 676-740 8,5-9,3 >1433 >18 160-183 20-23 -0.03 -0.20 350
YXG22H 0,93-0,97 9.3-9.7 676-740 8,5-9,3 >1990 >25 160-183 20-23 -0.03 -0.20 350
YXG24 0,95-1,02 9.5-10.2 692-764 8.7-9.6 >1433 >18 175-191 22-24 -0.03 -0.20 350
YXG24H 0,95-1,02 9.5-10.2 692-764 8.7-9.6 >1990 >25 175-191 22-24 -0.03 -0.20 350
YXG26M 1.02-1.05 10.2-10.5 541-780 6,8-9,8 636-1433 8-18 191-207 24-26 -0.03 -0.20 300
YXG26 1.02-1.05 10.2-10.5 748-796 9.4-10.0 >1433 >18 191-207 24-26 -0.03 -0.20 350
YXG26H 1.02-1.05 10.2-10.5 748-796 9.4-10.0 >1990 >25 191-207 24-26 -0.03 -0.20 350
YXG28M 1.03-1.08 10.3-10.8 541-796 6.8-10.0 636-1433 8-18 207-223 26-28 -0.03 -0.20 300
YXG28 1.03-1.08 10.3-10.8 756-812 9.5-10.2 >1433 >18 207-223 26-28 -0.03 -0.20 350
YXG28H 1.03-1.08 10.3-10.8 756-812 9.5-10.2 >1990 >25 207-223 26-28 -0.03 -0.20 350
YXG30M 1.08-1.10 10.8-11.0 541-835 6,8-10,5 636-1433 8-18 223-240 28-30 -0.03 -0.20 300
YXG30 1.08-1.10 10.8-11.0 788-835 9.9-10.5 >1433 >18 223-240 28-30 -0.03 -0.20 350
YXG30H 1.08-1.10 10.8-11.0 788-835 9.9-10.5 >1990 >25 223-240 28-30 -0.03 -0.20 350
YXG32M 1.10-1.13 11.0-11.3 541-844 6.8-10.6 636-1433 8-18 230-255 29-32 -0.03 -0.20 300
YXG32 1.10-1.13 11.0-11.3 812-844 10.2-10.6 >1433 >18 230-255 29-32 -0.03 -0.20 350
YXG32H 1.10-1.13 11.0-11.3 812-844 10.2-10.6 >1990 >25 230-255 29-32 -0.03 -0.20 350
YXG34M 1.13-1.16 11.3-11.6 835-884 10.5-11.1 636-1433 8-18 246-270 31-34 -0.03 -0.20 300
YXG34 1.13-1.16 11.3-11.6 835-884 10.5-11.1 >1433 >18 246-270 31-34 -0.03 -0.20 350
YXG34H 1.13-1.16 11.3-11.6 835-884 10.5-11.1 >1990 >25 246-270 31-34 -0.03 -0.20 350
Germahiya Kêm Sm2Co17, (SmEr)2(CoTm)17, SmCo 2:17 magnets
YXG22LT 0,94-0,98 9.4-9.8 668-716 8.4-9.0 >1194 >15 167-183 21-23 -0,015 -0.20 350

Neodymium MagnetNîşan û Taybetmendî:

Neodymium (NdFeB), Neo, an Neodymium Iron Boron magnetek cûrbecûr sepanên mîna motorên DC yên bê firçe, senzor û dengbêjan hene, ji ber taybetmendiyên wê yên berbiçav ên wekî taybetmendiyên magnetîkî yên bilind (di nav de înduksiyona mayî, hêza zorê, û hilbera enerjiyê ya herî zêde), bêtir vebijarkên polên magnetîkî û germahiya xebitandinê, di makînekirinê de hêsantir peydakirina gelek şekl û mezinahiyên berdest, hwd.

Sinif Induction Bermayî
Br
Coercivity
Hcb
Zordariya Navxweyî
Hcj
Hilbera Enerjiya herî zêde
(BH) max
Rev. Temp. Coef.
α(Br)
Rev. Temp. Coef.
β(Hcj)
Max Working Temp.
T kG kA/m kOe kA/m kOe kJ/m3 MGOe %/°C %/°C °C
N35 1.17-1.22 11.7-12.2 >868 >10.9 >955 >12 263-287 33-36 -0.12 -0.62 80
N38 1.22-1.25 12.2-12.5 >899 >11.3 >955 >12 287-310 36-39 -0.12 -0.62 80
N40 1,25-1,28 12.5-12.8 >907 >11.4 >955 >12 302-326 38-41 -0.12 -0.62 80
N42 1.28-1.32 12.8-13.2 >915 >11.5 >955 >12 318-342 40-43 -0.12 -0.62 80
N45 1,32-1,38 13.2-13.8 >923 >11.6 >955 >12 342-366 43-46 -0.12 -0.62 80
N48 1,38-1,42 13.8-14.2 >923 >11.6 >955 >12 366-390 46-49 -0.12 -0.62 80
N50 1.40-1.45 14.0-14.5 >796 >10.0 >876 >11 382-406 48-51 -0.12 -0.62 80
N52 1,43-1,48 14.3-14.8 >796 >10.0 >876 >11 398-422 50-53 -0.12 -0.62 80
N33M 1.13-1.17 11.3-11.7 >836 >10.5 >1114 >14 247-263 31-33 -0.11 -0.60 100
N35M 1.17-1.22 11.7-12.2 >868 >10.9 >1114 >14 263-287 33-36 -0.11 -0.60 100
N38M 1.22-1.25 12.2-12.5 >899 >11.3 >1114 >14 287-310 36-39 -0.11 -0.60 100
N40M 1,25-1,28 12.5-12.8 >923 >11.6 >1114 >14 302-326 38-41 -0.11 -0.60 100
N42M 1.28-1.32 12.8-13.2 >955 >12.0 >1114 >14 318-342 40-43 -0.11 -0.60 100
N45M 1,32-1,38 13.2-13.8 >995 >12.5 >1114 >14 342-366 43-46 -0.11 -0.60 100
N48M 1,36-1,43 13.6-14.3 >1027 >12.9 >1114 >14 366-390 46-49 -0.11 -0.60 100
N50M 1.40-1.45 14.0-14.5 >1033 >13.0 >1114 >14 382-406 48-51 -0.11 -0.60 100
N33H 1.13-1.17 11.3-11.7 >836 >10.5 >1353 >17 247-263 31-33 -0.11 -0.58 120
N35H 1.17-1.22 11.7-12.2 >868 >10.9 >1353 >17 263-287 33-36 -0.11 -0.58 120
N38H 1.22-1.25 12.2-12.5 >899 >11.3 >1353 >17 287-310 36-39 -0.11 -0.58 120
N40H 1,25-1,28 12.5-12.8 >923 >11.6 >1353 >17 302-326 38-41 -0.11 -0.58 120
N42H 1.28-1.32 12.8-13.2 >955 >12.0 >1353 >17 318-342 40-43 -0.11 -0.58 120
N45H 1,32-1,36 13.2-13.6 >963 >12.1 >1353 >17 326-358 43-46 -0.11 -0.58 120
N48H 1,36-1,43 13.6-14.3 >995 >12.5 >1353 >17 366-390 46-49 -0.11 -0.58 120
N33SH 1.13-1.17 11.3-11.7 >844 >10.6 >1592 >20 247-263 31-33 -0.11 -0.55 150
N35SH 1.17-1.22 11.7-12.2 >876 >11.0 >1592 >20 263-287 33-36 -0.11 -0.55 150
N38SH 1.22-1.25 12.2-12.5 >907 >11.4 >1592 >20 287-310 36-39 -0.11 -0.55 150
N40SH 1,25-1,28 12.5-12.8 >939 >11.8 >1592 >20 302-326 38-41 -0.11 -0.55 150
N42SH 1.28-1.32 12.8-13.2 >987 >12.4 >1592 >20 318-342 40-43 -0.11 -0.55 150
N45SH 1,32-1,38 13.2-13.8 >1003 >12.6 >1592 >20 342-366 43-46 -0.11 -0.55 150
N28UH 1.02-1.08 10.2-10.8 >764 >9.6 >1990 >25 207-231 26-29 -0.10 -0.55 180
N30UH 1.08-1.13 10.8-11.3 >812 >10.2 >1990 >25 223-247 28-31 -0.10 -0.55 180
N33UH 1.13-1.17 11.3-11.7 >852 >10.7 >1990 >25 247-271 31-34 -0.10 -0.55 180
N35UH 1.17-1.22 11.7-12.2 >860 >10.8 >1990 >25 263-287 33-36 -0.10 -0.55 180
N38UH 1.22-1.25 12.2-12.5 >876 >11.0 >1990 >25 287-310 36-39 -0.10 -0.55 180
N40UH 1,25-1,28 12.5-12.8 >899 >11.3 >1990 >25 302-326 38-41 -0.10 -0.55 180
N28EH 1.04-1.09 10.4-10.9 >780 >9.8 >2388 >30 207-231 26-29 -0.10 -0.55 200
N30EH 1.08-1.13 10.8-11.3 >812 >10.2 >2388 >30 223-247 28-31 -0.10 -0.55 200
N33EH 1.13-1.17 11.3-11.7 >836 >10.5 >2388 >30 247-271 31-34 -0.10 -0.55 200
N35EH 1.17-1.22 11.7-12.2 >876 >11.0 >2388 >30 263-287 33-36 -0.10 -0.55 200
N38EH 1.22-1.25 12.2-12.5 >899 >11.3 >2388 >30 287-310 36-39 -0.10 -0.55 200
N28AH 1.04-1.09 10.4-10.9 >787 >9.9 >2785 >35 207-231 26-29 -0.10 -0.47 230
N30AH 1.08-1.13 10.8-11.3 >819 >10.3 >2785 >35 223-247 28-31 -0.10 -0.47 230
N33AH 1.13-1.17 11.3-11.7 >843 >10.6 >2785 >35 247-271 31-34 -0.10 -0.47 230

Plating bo Magnets:

Layera Çêkirinê Reng Tîpîkî Thickness
µm
SST
Seet
PCT
Seet
Germahiya xebatê.
°C
Taybetmendiyên Serlêdana Tîpîkî
Nickel Ni+Cu+Ni, Ni+Ni Bright Silver 10-20 > 24-72 > 24-72 <200 Bi gelemperî tê bikaranîn magnets Industrial
Şîn Spî Zinc Zn Şîn Spî 8-15 > 16-48 >12 <160 Tenik û erzan Magnetên motora elektrîkê
Reng Zinc 3+Cr Rengê Zn Rengê Ronahî 5-10 >36-72 >12 <160 Adhesion nazik û baş Magnetên Speaker
Nîkelê kîmyewî Ni+Ni Kîmyayî Zîv tarî 10-20 > 24-72 >16 <200 Stûrahiya yekgirtî Electronics
Epoxy Epoxy, Zn+Epoxy Reş / Gewr 10-25 >96 >48 <130 Berxwedana korozyonê ya nerm û baş Automotive
NiCuEpoxy Ni+Cu+Epoxy Reş / Gewr 15-30 >72-108 >48 <120 Berxwedana korozyonê ya nerm û baş magnets motor Linear
Fosfatkirin Fosfatkirin Gewrê Ronahî 1-3 —- —- <240 Parastina Demkî Magnetên motora elektrîkê
Pasîvasyon Pasîvasyon Gewrê Ronahî 1-3 —- —- <240 Parastina Demkî Magnetên servo motor
Parylene Parylene Zelal 3-10 >24 —- <150 Tensile, sivik û pêbaweriya bilind Leşkerî, Aerospace
Lastîk Lastîk Reş 500 >72-108 —- <130 Berxwedana sirûştî û korozyonê ya baş Girtina magnetan

Ewlehiya Magnet:

Magnatasên erdê yên hindik an pergalên magnetîkî zehf bi hêz in, ji ber vê yekê tedbîrên ewlehiyê yên jêrîn divê ji hemî personelên ku dikarin wan bikar bînin, hilgirin, an jî pêvajo bikin da ku ji zirara kesane an zirara magnetan dûr nekevin.

Dema ku ew bi hevûdu re an bi materyalên ferromagnetic re têkevin têkiliyê, pê ewle bin ku magnetên erdên kêm ên magnetîzekirî di bin kontrolê de bin. Girîng e ku meriv camên ewlehiyê û kelûmelên din ên parastinê yên guncan dema ku bi magnetên mezin ve mijûl dibin li xwe bikin. Ji bo parastina destên xwe girtina destan jî tê pêşniyar kirin.

Metalên ferromagnetîk ji qada xebatê dûr bigirin. Dema ku bi magnetan re dixebitin baldar bin. Heke hûn di bin bandora alkol, narkotîk, an madeyên kontrolkirî de ne bi magnetên magnetîzekirî re bixebitin.

Amûr û amûrên elektronîkî yên hesas dibe ku kalibrasyonê biguhezînin an ji hêla zeviyek magnetîkî ya hêzdar ve zirarê bibînin. Her gav magnetên magnetîzekirî ji amûrên elektronîkî yên hesas dûrek ewledar dûr bigirin. Ger kesek pacemaker li xwe bike divê hişyariyek taybetî were kirin, ji ber ku zeviyên magnetîkî yên bihêz dikarin zirarê bidin elektronîkên hundurê pacemakers.

Tu carî magnetan daqurtînin û magnetan li ber destên zarok an mezinên astengdar ên derûnî nehêlin. Ger magnets werin daqurtandin, tavilê bi doktor re şêwir bikin û/an jî tavilê li bal bijîşkî bigerin.

Magnetayên erdê yên hindik dibe ku bi têkiliya di destgirtinê de çirûskan çêkin, nemaze dema ku destûr bidin ku bandorê li hev bikin. Di atmosferên teqemenî de tu carî magnetên erdê yên nadir negirin ji ber ku çirûsk dikare wê atmosferê bişewitîne.

Toza erda hindik şewitî ye; dema ku toz zuwa be, şewitandina xwebexş dikare çêbibe. Ger hûrkirin, her gav magnetên hûrkirinê şil bikin da ku xwe ji şewitandina xwebexş a swarfê qirkirinê dûr bixin. Qet hişk neke. Dema ku magnetan hûr dikin, pê ewle bin ku hewaya têra xwe hebe. Hewl nedin ku magnetan bi karanîna amûrên konvansiyonel makîne bikin, ji ber ku ev dikare çîp û şikestin çêbike. Her tim camên ewlehiyê li xwe bikin.

Her gav toza erdê kêm an çîpên hûrkirî di konteynerên tije av an jî atmosferên bêhêz ên bi hermetîkî vegirtî de hilînin da ku pêşî li şewitandina xwebexş bigirin.

Her gav toza erdê kêm bi baldarî bavêjin. Metirsiya şewatê nekin. Rakirina magnetên magnetîzekirî divê were kirin da ku di dema hilgirtinê de zirarê neyê girtin.